2036 Aluminum foil

2036 aluminum this is an early application of a kind of hard aluminum, commonly known as standard hard aluminum, with moderate strength, annealing, quenching and hot state plasticity is good, heat treatment can be strengthened, quenching and natural aging state in use, spot welding weldability is good.
2036 aluminum alloy features: high strength, a certain heat resistance, can be used for working parts below 150℃.
The strength of 2036 alloy is higher than that of 7075 alloy.

5052 Aluminum foil

1100 aluminum alloy is 99.0% ordinary industrial pure aluminum.
Heat treatment can not be strengthened; Low strength, but good ductility, formability, weldability and corrosion resistance;
After anodic oxidation, the corrosion resistance can be further improved and a beautiful surface can be obtained.

1070 Aluminum foil

1070 aluminum has high plasticity, corrosion resistance, electrical conductivity and good thermal conductivity, but low strength, not through heat treatment to strengthen, cutting is not good, can accept contact welding, gas welding.
Make use of its advantages to manufacture some structural parts with specific performance, such as aluminum foil gaskets and capacitors, electronic tube isolation net, wire, cable protection sleeve, net, wire core and aircraft ventilation system parts and decorative parts.

1100 Aluminum foil

1100 aluminum alloy is 99.0% ordinary industrial pure aluminum.
Heat treatment can not be strengthened; Low strength, but good ductility, formability, weldability and corrosion resistance;
After anodic oxidation, the corrosion resistance can be further improved and a beautiful surface can be obtained.

6061-T6 Aluminum foil

The main alloying elements in 6061 alloy are magnesium and silicon, which have moderate strength, good corrosion resistance, weldability and good oxidation effect.
Widely used in various industrial structural parts requiring a certain strength and high antibiotic corrosion, its main chemical composition: Cu:0.15-0.4; Si: 0.4-0.8; Fe: 0.7 -; Mn: 0.15; Mg: 0.8-1.2; Zinc: 0.25; Cr: 0.04-0.35; Ti: 0.15 -; 6061 aluminum plate its state T6 and T651 difference is that in general, T6 internal stress will be relatively large, processing will be deformed, the most suitable for processing state should be T651, he is on the basis of T6 tensile, eliminate internal stress.

2036 Aluminum pipe

2036 aluminum this is an early application of a kind of hard aluminum, commonly known as standard hard aluminum, with moderate strength, annealing, quenching and hot state plasticity is good, heat treatment can be strengthened, quenching and natural aging state in use, spot welding weldability is good.
2036 aluminum alloy features: high strength, a certain heat resistance, can be used for working parts below 150℃.
The strength of 2036 alloy is higher than that of 7075 alloy.

6082 Aluminum foil

6082 is a heat-treatable alloy with good formability, weldability, machinability and corrosion resistance.
It also has moderate strength and can maintain good operability after annealing.
It is mainly used in mechanical structure, including bars, plates, pipes and profiles.

1070 Aluminum pipe

1070 aluminum has high plasticity, corrosion resistance, electrical conductivity and good thermal conductivity, but low strength, not through heat treatment to strengthen, cutting is not good, can accept contact welding, gas welding.
Make use of its advantages to manufacture some structural parts with specific performance, such as aluminum foil gaskets and capacitors, electronic tube isolation net, wire, cable protection sleeve, net, wire core and aircraft ventilation system parts and decorative parts.